General Alloy Overview

ASTM

Application Examples

Industry Examples

Tempers

Available Forms

Constant (Temper - Independent) Properties

ParameterValue
Solidus, °F (°C)1950 (1065)
Density, dwt/in3 (g/cm3)125.0 (11.9)
Electrical Resistivity, Ω-cmf (µΩ-cm)220 (36.6)
Electrical Conductivity, %IACS5
Thermal Conductivity, Btu/hr-ft-°F (W/m-K)19.5 (11.3)
ParameterValue
Coefficent of Thermal Expansion, /°F (/K)7.5E-06 (1.4E-05)
Specific Heat Capacity, Btu/lb-°F (J/g-K) 0.064 (0.268)
Elastic Modulus, Msi (GPa)17.9 (123.09)
Shear Modulus, Msi (GPa)6.5 (44.9)

Temper Dependent Properties

Intermediate Wire

AnnealedStress Relieved
0.2% Offset Yield Strength, ksi (MPa)120 (827)137 (947)
Ultimate Tensile Strength, ksi (MPa)106 (733)142 (982)
Elongation to Failure, %3519
Knoop Microhardness, HK100213302
Electrical Resistivity, Ω-cmf (μΩ-cm)220 (37)-
Thermal Conductivity, Btu/hr-ft-°F (W/m-K)11.3 (19.5)-