Temper Independent Properties

ParameterValueValue 2
Solidus, °F (°C)2580(1415)
Liquidus, °F (°C)2750(1510)
Melting Range, °F (°C)170(95)
Density, dwt/in³­ (g/cm³)185(17.5)
Specific Heat Capacity, Btu/lb·°F, (J/g·K)0.037(0.15)
Coefficient of Thermal Expansion, /°F (/K)6.8E-06(1.2E-05)
Thermal EMF vs Pt, μV/°F (μV/°C)-8.1(-14.5)
Emissivity.27
ParameterValueValue 2
Thermal Conductivity, (Btu/hr·ft·°F) W/m·k15(25)
Temperature Coefficient of Resistance, /°F (/K)1.75E-04(3.1E-04)
Electrical Resistivity, Ω·cmf (µΩ·cm)175(30)
Electrical Conductivity, %IACS6
Elastic Modulus, Msi (GPa)20(140)
Shear Modulus, Msi (GPa)7.2(50)
Poissons Ratio.38
Nobility, %100

Biocompatibility and Medical Imaging Properties

ParameterValue
Cytotoxicity (ISO 10993-5)Pass
Intracutaneous Study (ISO 10993-10)Pass
ParameterValue
Systemic Toxicity (ISO 10993-11)Pass

Temper Dependent Properties

Cold Worked - Rod .100'' - .300'' diameter

ParameterNominalMin
NominalMin
0.2% Offset Yield Strength, ksi (MPa)110 (760)83 (572)
Tensile Elongation to Failure, %71
Vickers Microhardness, HV100270N/A
ParameterNominalMin
NominalMin
Ultimate Tensile Strength, ksi (MPa)130 (900)110 (760)
Knoop Microhardness, HK100280230