Alloy 8010

General Alloy Overview

ASTM

N/A

Application Examples

Medical Devices

Industry Examples

Dental

Tempers

Cold Worked

Availible Forms

Rod

Biocompatibility and Medical Imaging Properties

Select compatibility testing for biomaterials applications has been completed and is available upon request

Temper Independent Properties

ParameterValueValue 2
Solidus, °F (°C)1920(1050)
Liquidus, °F (°C)2210(1210)
Melting Range, °F (°C)290(160)
Density, dwt/in³­ (g/cm³)115(10.7)
Specific Heat Capacity, Btu/lb·°F, (J/g·K)0.063(0.265)
Coefficient of Thermal Expansion, /°F (/K)7.1×10-6(13×10-5)
Thermal EMF vs Pt, μV/°F (μV/°C)-7.7(-14)
Emissivity0.233
ParameterValueValue 2
Thermal Conductivity, (Btu/hr·ft·°F) W/m·k8.0(14)
Temperature Coefficient of Resistance, /°F (/K)
Electrical Resistivity, Ω·cmf (µΩ·cm)310(52)
Electrical Conductivity, %IACS3.3
Elastic Modulus, Msi (GPa)18(125)
Shear Modulus, Msi (GPa)6.7(45)
Poissons Ratio0.38
Nobility, %82.4

Temper Dependent Properties

Cold Worked - Rod 0.100 - 0.300 in. (2.5 - 7.6 mm) diameter

ParameterNominalMin
NominalMin
0.2% Offset Yield Strength, ksi (MPa)140 (965)(N/A)
Tensile Elongation to Failure, %54
Vickers Microhardness, HV(N/A)
ParameterNominalMin
NominalMin
Ultimate Tensile Strength, ksi (MPa)175 (1200)165 (1140)
Knoop Microhardness, HK350

† - Values containing † are available upon request​

Contact A Specialist